What is undercut welding? Undercut is a groove melted into the base metal along the toe of a weld, or at the root, that weld metal did not fill. It sits in the parent metal beside the bead, not in the bead itself. Before anyone discusses whether it is acceptable, a QC sheet should name it as undercut, say where it is, and separate it from underfill, overlap and arc strikes, which look similar in photos but are different conditions.
The distinction matters because each condition has its own cause, its own effect on the joint, and often its own acceptance treatment. A photo labelled “bad weld” gives a supplier nothing to act on. A photo labelled “undercut at the upper toe of the tube-to-plate fillet, about one third of the weld length” does.
This guide is for importers, quality managers and product teams who review welded metal bathroom and storage hardware. Koitor Hardware is a family-owned China OEM manufacturer that uses TIG, laser and resistance welding on towel racks, shower caddies, hooks and wire products. We explain identification; acceptance belongs to the specification.
Acceptance on thin stainless hardware is covered in the live guide to stainless weld undercut acceptance on thin sheet. This page answers the earlier question: what undercut is, and how to tell it apart from its neighbours.
What is undercut welding, in plain terms?
Undercut is a channel along the edge of a weld where the arc or beam melted the base metal and the molten metal flowed away into the weld pool without refilling the edge. The result is a local loss of base metal thickness right at the weld toe. It may be continuous or intermittent along the weld.
El TWI review of geometric shape imperfections describes undercut as an irregular groove at the toe of a run in the parent metal. It notes that undercut can appear at the surface of a completed joint and at the toes of individual passes in multi-pass welds.
International terminology groups weld imperfections into families. ISO 6520-1 classifies geometric imperfections in fusion welding, including shape imperfections such as undercut, overlap and incompletely filled groove. Using that shared vocabulary helps buyers and suppliers mean the same thing.
On hardware, undercut most often appears where a tube meets a plate or flange, where a wire meets a frame, or along fillet welds on brackets. Thin walls make it more visible and potentially more significant, because the groove removes a larger share of the wall.
The defining feature is location. Undercut is in the base metal at the edge of the weld. If the dip is in the weld face itself, the condition is more likely underfill or an incompletely filled groove. If weld metal has rolled over the base metal without fusing, it is overlap. If a scar sits away from the weld, it may be an arc strike.
Can undercut occur on the root side of a weld?
Yes. On joints welded from one side, such as some tube or pipe joints, the root side can show a groove at the root toe. It is often harder to see because the root side may be inside a tube. A QC sheet should state whether the observation was on the face side, the root side, or both.
How is undercut different from underfill, overlap and arc strike?
Undercut removes base metal at the weld toe. Underfill leaves the weld face below the required profile. Overlap lays weld metal over the base metal surface without fusion. An arc strike is a localised melt scar outside the intended weld. They can coexist on one joint, so each should be named separately with its location.
Underfill is the most common confusion. The live weld underfill guide explains that underfill is about the weld face sitting below the profile the joint design requires. The groove is in the weld, not beside it. Undercut, by contrast, leaves the weld face intact but cuts into the parent metal edge.
Overlap is almost the opposite visually. Weld metal flows onto the base metal surface beyond the toe and sits there unfused, creating a lip. The live weld overlap guide covers how that lip forms and why it can hide a notch underneath.
Arc strikes are separate events. They are small melt spots where an arc touched the surface outside the weld, often from a torch or electrode contact. The live arc strike guide explains why they matter on stainless and how to describe them.
| Condición | Where it sits | What it looks like | Covered in |
|---|---|---|---|
| — | — | — | — |
| Undercut | Base metal at the weld toe or root | A groove or channel beside the bead, below the original surface | This page; acceptance on thin stainless in the live acceptance guide |
| Underfill | Weld face | Weld surface below the required profile, a dip in the bead | Weld underfill |
| Overlap | Base metal surface beyond the toe | Weld metal rolled over the surface without fusing, forming a lip | Weld overlap |
| Arc strike | Base metal away from the weld | A small melt spot or scar outside the intended joint | Arc strike |
| Porosity | Inside or on the weld metal | Round pores or pinholes in the bead | Batch guide on porosity in welding |
The table is a starting point for describing a photo, not an acceptance tool. Two conditions can occur together. For example, a groove at one toe and overlap at the other can appear on the same fillet when the torch angle favours one side. Each should be recorded with its location.

Why does undercut matter on welded hardware?
Undercut matters because it reduces the base metal section at the weld toe and creates a notch where stresses concentrate. On thin tube and sheet, a small groove can remove a meaningful share of the wall. Whether that matters depends on the depth, length, location, load direction and the criteria the specification applies.
Load direction is important. A groove running along a weld that carries load across it acts differently from one parallel to the main stress. A towel bar bracket loaded by a hanging towel and the occasional pull sees different stresses at its upper and lower toes. The acceptance guide explains why location and load direction belong in the review.
Fatigue is the other concern. Repeated loading concentrates at notches, and undercut is a notch. For hardware that sees repeated use, such as hooks, rails and fold-down shelves, a toe groove at a highly stressed point deserves more attention than the same groove on a lightly loaded tack.
Appearance matters too. On polished or brushed stainless, a groove along a visible weld can catch light and dirt. On powder-coated steel, a sharp toe groove may affect how coating covers the edge. Those are cosmetic and coating questions, but they are real for retail products.
Corrosion is a further consideration on stainless. A sharp groove can collect moisture, soap residue and chloride deposits in a bathroom. Whether that becomes a corrosion problem depends on the grade, the surface condition after welding and cleaning, and the service environment. It is a reason to describe undercut carefully, not a prediction that it will corrode.
Assembly can also be affected. Where a welded bracket mates with a wall plate, cover or escutcheon, a groove at the toe may change how the parts seat, or leave a visible gap. Those fit questions belong in the sample review, alongside the weld appearance.
None of this means every groove is a reject. Most weld quality standards permit some undercut, with limits that depend on quality level and thickness. The point of identification is to describe the condition accurately so the right criteria can be applied, not to decide the outcome in advance.
Multi-pass welds add another layer. Undercut at the toe of an intermediate pass can trap slag or prevent the next pass from fusing properly, which turns a shape imperfection into an internal one. Most hardware welds are single-pass on thin material, but heavier brackets or bases may use more than one run, so the QC plan should note it.
Does undercut always need repair?
No. Whether undercut needs repair depends on the specified acceptance criteria, the depth and length measured, the location and the part’s function. Some criteria allow limited undercut with a smooth transition. A repair method, if needed, should follow the welding procedure and the customer’s requirements, not a generic rule.
What should a QC sheet record when undercut is suspected?
Record the joint, the toe or root affected, the length and whether it is continuous or intermittent, how depth was assessed, the lighting and magnification used, and the acceptance reference. Add a photo with a scale reference and raking light. That record lets the supplier act and lets a reviewer apply the criteria.
Joint identification comes first. Use the weld numbering on the drawing if there is one, or describe the joint clearly: for example, the upper fillet between the left arm tube and the wall plate. The live guide on how to read welding symbols explains how drawings identify joints and weld types.
Toe or root comes next. Say which side of the bead the groove is on, and whether it is on the face side or root side. On a fillet weld, the upper toe on a vertical member is a common location.
Length and continuity describe extent. Record whether the groove runs the full weld length, a portion, or appears in short intermittent sections. Many criteria treat continuous and intermittent undercut differently.
Depth assessment is the hardest part. Visual inspection with raking light shows presence; measuring depth needs a suitable gauge or other method. The live guide on how to use a fillet weld gauge explains what common weld gauges measure. Record the tool used, so the figure can be repeated.
Lighting and magnification affect what is seen. Flat overhead light can hide a shallow groove. Low-angle light along the weld makes it cast a shadow. Record the conditions, especially when comparing reports from different inspectors.
Consistent wording across reports helps trend analysis. If one inspector writes “toe groove”, another “undercut” and a third “edge burn”, a later review cannot tell whether three lots had the same problem. Agreeing the term and the fields once, then using them every time, makes the record useful beyond a single shipment.
- Joint identified by drawing weld number or clear description.
- Toe or root side stated, and face or root surface stated.
- Length recorded, with continuous or intermittent noted.
- Depth assessment method and tool named, with the reading if measured.
- Lighting angle and magnification recorded.
- Photo with scale reference taken under raking light.
- Acceptance reference named: drawing, customer specification or quality level.
How do inspection methods change what undercut you find?
The method determines what can be seen and measured. Unaided visual inspection finds obvious grooves; raking light and magnification find shallow ones; depth gauges and profile measurement quantify them; sectioning shows the true profile but destroys the sample. A report should name the method, because each one answers a slightly different question.
Visual inspection is the usual first step, and many criteria for hardware rely on it. Its weakness is consistency. Two inspectors under different lighting can disagree about whether a shallow groove exists. Agreeing a lighting arrangement and magnification level, and using reference photos, makes visual results more repeatable.
Depth measurement needs a tool that fits the joint. Some weld gauges include an undercut depth feature; on small hardware joints, access can be limited by tube curvature or nearby features. Where a gauge cannot sit properly, the report should say so rather than record a figure the tool could not reliably produce.
Profile replication is an option for small or hard-to-reach toes. A replica material pressed into the joint captures its shape, which can then be examined or sectioned. It is slower than a gauge but avoids cutting the part. It suits disputes where both sides need to see the same profile.
Sectioning gives the clearest answer. Cutting through the joint, polishing and sometimes etching the face shows the toe profile, the groove depth relative to the wall, and whether other conditions sit nearby. It destroys the sample, so it is usually reserved for qualification, disputes or periodic audits rather than routine lots.
Hidden root sides need a decision. Inside a tube, the root toe may be inaccessible without cutting. If the root side matters to the specification, the inspection plan should say how it will be examined, for example by sectioning a sample per lot. Otherwise the report should state that only the face side was inspected.
Finishing can hide or change undercut. Grinding and polishing after welding may blend a shallow groove, or may remove base metal around it and make it look worse. Powder coating can partly fill a shallow groove visually. Inspection before finishing, after finishing, or both, should be stated in the plan.
Does undercut terminology apply to resistance welds?
Undercut is mainly used for arc and beam fusion welds, where a molten pool forms along a toe. Resistance spot and projection welds on wire and sheet form a different joint geometry, and their imperfections are usually described in other terms, such as indentation or expulsion. Using the right vocabulary for the process avoids confused reports.
Where should undercut acceptance be decided?
Acceptance belongs to the criteria named on the drawing or in the customer’s specification, such as a quality level in ISO 5817 or another code the customer applies. This page does not print numeric limits, because they depend on the standard, quality level, thickness and joint type that the specification selects.
Many buyers ask for a single number. The difficulty is that limits change with material thickness, the chosen quality level, and whether the weld is a butt or fillet. A number taken from one context can be too strict or too loose for another. The live thin sheet acceptance guide explains which factors the review should consider for stainless hardware.
If the drawing is silent, the right response is to agree criteria before production, not after a dispute. That agreement can name a standard and quality level, or describe the requirement in the customer’s own terms with photos of acceptable and unacceptable examples.
Process causes are a separate discussion. General welding knowledge associates undercut with high arc voltage or long arc length, excessive current, high travel speed and torch angle. Those are inferences about welding in general, not a diagnosis of any particular lot. Confirming a cause on a specific product needs the welding records and a review of the procedure.
From Koitor’s manufacturing side, TIG, laser and resistance welding each behave differently at the toe. Laser welds on thin stainless can be narrow with small heat input; TIG welds on tube-to-plate joints depend heavily on torch angle and filler addition. Matching the acceptance criteria to the actual process and joint makes the review fair to both sides.
Sample approval is the practical moment to settle these points. When a buyer approves a welded sample, recording the weld appearance with photos under agreed lighting creates a reference. Later lots can be compared against that reference using the same terms, which is fairer than comparing them against memory or an unspecified ideal.
Where a buyer has its own visual standard, sharing marked-up photos of acceptable and unacceptable toes is often more useful than text alone. It shows exactly which groove depth, length and finish the buyer means, and it gives the welding team a target they can check during production.

Buyer checklist before calling a weld undercut
- The groove is in the base metal at the toe or root, not in the weld face.
- Underfill, overlap and arc strikes have been ruled out or recorded separately.
- The joint, side and surface are identified.
- Length and continuity are recorded.
- Depth has been assessed with a named method or tool.
- A photo under raking light with a scale reference is attached.
- The acceptance reference is named before a decision is made.
- Any cause discussion is labelled as inference until welding records are reviewed.
Preguntas frecuentes
What is undercut in welding?
Undercut is a groove melted into the base metal at the toe or root of a weld that was not filled by weld metal. It reduces the local base metal thickness and forms a notch beside the bead. It differs from underfill, which is a weld face below the required profile.
Is undercut the same as underfill?
No. Undercut is in the base metal beside the weld. Underfill is in the weld face, which sits below the profile the joint design requires. Both can occur on the same joint, so each should be named and located separately on a QC sheet.
How much undercut is acceptable?
It depends on the acceptance criteria the specification names, such as a quality level in a weld standard, plus material thickness and joint type. This page does not give numeric limits, because a figure from one context can be wrong for another. Agree the criteria before production.
How can undercut be seen on a polished stainless part?
Use low-angle raking light along the weld and magnification. A groove casts a shadow that overhead light hides. Photograph under the same conditions with a scale reference, so the observation can be reviewed and repeated by another inspector.
What causes undercut?
General welding knowledge links undercut to high arc voltage, long arc length, excessive current, high travel speed and torch angle. Those are general process inferences. A cause on a specific lot should be confirmed against welding records and the procedure, not assumed from a photo.
Can grinding remove undercut?
Blend grinding is sometimes used to smooth a shallow toe groove into a gradual transition, but it removes more base metal in the process. Whether it is allowed, and how much thickness may remain afterwards, depends on the specification and the welding procedure. It should not be treated as a default fix.
Trabaja con Koitor Hardware
Review weld wording on a hardware drawing
Send the drawing, the weld callouts and any acceptance criteria your customer specifies. We can review whether the wording names discontinuities, locations and the acceptance reference clearly enough to be applied to welded hardware parts. We do not certify welders or act as a welding inspector.
OEM / MARCA BLANCA
Convierte esta guía de abastecimiento en un resumen del producto
Indícanos el producto que deseas, el tamaño, el acabado, la cantidad del pedido y los requisitos de embalaje. Tu equipo recibirá un análisis práctico de la viabilidad de fabricación antes de recibir el presupuesto.