Lack of fusion in welding is an unbonded interface where weld metal did not melt into and join the base metal, or did not join a previous weld pass. It can sit along a joint sidewall, between passes, or at the root.
Before anyone calls a weld acceptable or rejected, a QC sheet should name the condition as lack of fusion, say which interface is affected, state how it was found, and keep it separate from lack of penetration, porosity and undercut.
That separation matters because these conditions are often discussed together and confused in photos. Lack of fusion is a bonding failure at an interface. Lack of penetration is a depth shortfall at the root. Porosity is a gas void. Undercut is a groove at the toe. Each has different causes, different detection methods and different acceptance treatment.
This guide is for importers, quality managers and product teams who review welded metal bathroom and storage hardware. Koitor Hardware is a family-owned China OEM manufacturer that uses TIG, laser and resistance welding on towel racks, shower caddies, wire baskets, hooks and racks. We explain identification; acceptance belongs to the specification.
Related batch guides cover what is undercut welding et what is porosity in welding. The live weld underfill guide covers a low weld face. This page focuses on the unbonded interface.
What is lack of fusion in welding?
Lack of fusion means the weld metal and the surface it should have joined stayed separate along some length. The arc or beam did not melt that surface enough, or molten metal flowed onto it without bonding. The result is a thin, flat discontinuity, often invisible from outside, lying along the line where fusion should have happened.
Le TWI job knowledge article on lack of sidewall and inter-run fusion describes two main forms. Weld metal can fail to fuse with the sidewall of the joint, or fail to fuse with a previously deposited bead in a multi-pass weld. Root fusion failures are a third location.
Sidewall lack of fusion sits along one face of a groove or fillet. On a fillet weld joining a tube to a plate, it might lie along the tube surface while the plate side fused properly. From outside, the bead can look normal, because the problem is under the visible surface.
Inter-run lack of fusion occurs between passes. Most thin hardware welds are single-pass, but heavier brackets, bases and frames may use more than one run. If a later pass sits on an earlier one without melting into it, an unbonded layer forms inside the weld.
Root lack of fusion sits at the bottom of the joint. One side of the root may fuse while the other does not. This is closely related to lack of penetration, which is why the two are often confused and why the next section treats them separately.
Standard terminology groups these conditions together. ISO 6520-1 classifies lack of fusion and lack of penetration in the same family of geometric imperfections in fusion welding, then subdivides them by location. Using those terms helps buyers and suppliers describe the same thing.
Resistance welds use different terms again. Spot and projection welds on wire and sheet join parts through a nugget formed between them. A weak or missing nugget is usually described as insufficient nugget size or a cold weld, and checked with peel, chisel or other destructive tests in the resistance welding procedure. The bonding idea is similar, but the vocabulary and tests differ.
For wire baskets and grids, that distinction matters in reports. Calling a broken wire cross joint “lack of fusion” may be understandable shorthand, but the resistance welding records and test method are what the supplier will check. Naming the process avoids sending the investigation to arc welding parameters that were never used.
Why is lack of fusion hard to see?
Because it is usually flat and internal. A pore is rounded and may break the surface; undercut is visible at the toe. Lack of fusion often lies along a buried interface with weld metal covering it. Unless it breaks the surface at a toe or root, visual inspection may not reveal it at all.
How is lack of fusion different from lack of penetration?
Lack of fusion is a failure to bond at an interface. Lack of penetration is a failure of the weld to reach the required depth through the joint, leaving the root unfilled. A weld can penetrate fully yet have a sidewall that did not fuse, or fuse well on its faces yet stop short of the root.
Le TWI article on incomplete root fusion or penetration draws the root distinction clearly. Incomplete root fusion is when the weld fails to fuse one side of the joint at the root. Incomplete root penetration is when both sides of the root region remain unfused because the weld did not reach that far.
For buyers, the practical difference is what the drawing asks for. A weld symbol or note may specify the required penetration or effective throat. Lack of penetration means that requirement was not met. Lack of fusion means the weld that is there did not bond along some surface. Both reduce the effective joint, but in different ways.
Laser welds on thin stainless show the penetration question clearly. The live guide on laser weld penetration verification explains how penetration is evidenced on that route. Lack of fusion can also occur in laser welds, for example where joint fit-up leaves a gap the beam does not bridge.
| Condition | What failed | Where it sits | How it is usually found |
|---|---|---|---|
| — | — | — | — |
| Lack of sidewall fusion | Bonding between weld metal and joint face | Along a groove or fillet sidewall | Section, macro-etch, ultrasonic or radiographic methods; sometimes at a surface toe |
| Lack of inter-run fusion | Bonding between weld passes | Inside multi-pass welds | Section or internal examination |
| Incomplete root fusion | Bonding at one side of the root | Root of the joint | Root-side visual if accessible, section, internal examination |
| Lack of penetration | Weld depth short of the required root | Root region, both sides unfused | Root-side visual if accessible, section, internal examination |
| Porosity | Gas void in weld metal | Within or on weld metal | Visual for surface pores; section or radiography for internal |
| Undercut | Base metal groove at toe | Outside surface at the toe | Visual with raking light; depth gauge |
The table shows why method matters. A visual inspection report can speak confidently about undercut and surface porosity, but it usually cannot clear a weld of lack of fusion. That is an examination-method question, not a judgement about the inspector.

How is lack of fusion different from porosity, undercut and underfill?
Lack of fusion is a planar, unbonded interface. Porosity is rounded gas cavities in weld metal. Undercut is a groove in the base metal at the toe. Underfill is a weld face below the required profile. They can coexist, so each should be recorded with its own name, location and observation method.
Porosity is the most common confusion in sections. A polished slice may show both round voids and a dark line along a fusion boundary. The round voids are pores; the line is lack of fusion. Recording both separately lets the supplier investigate each, because their general causes differ.
Undercut and lack of fusion can be linked at the surface. A groove at the toe sometimes sits beside a toe where fusion was poor. The batch undercut guide explains how to describe the groove. If a section shows the weld did not bond beneath that toe, that is a separate observation.
Underfill relates to quantity of weld metal, not bonding. A weld can be fully fused but too small, or correctly sized but unfused along one side. The live underfill guide explains the profile question; this page explains the bonding question.
Slag inclusions are another neighbour in flux-based processes. Trapped slag can sit along a fusion boundary and look similar to lack of fusion in a section. Trapped slag is solid material; lack of fusion is an unbonded gap. Many hardware welds use TIG or laser processes that do not produce slag, but heavier fabrication sometimes uses flux processes.
Cracks are a further neighbour worth keeping apart. A crack is a fracture through metal, often with a sharp, irregular path, while lack of fusion follows the line where two surfaces should have joined. In a section, a crack may cross the fusion boundary or run through weld metal. Recording the path helps the reviewer decide which family the indication belongs to.
Can a weld look perfect and still have lack of fusion?
Yes. A smooth, well-shaped bead says little about bonding underneath. Molten metal can flow over a cold sidewall and solidify against it without fusing. That is why specifications that care about fusion name an examination method beyond visual inspection, or require sectioned samples.
How is lack of fusion detected?
Detection depends on where the unbonded interface lies and what the specification requires. Visual inspection finds only surface-breaking cases. Penetrant or magnetic particle testing can reveal fine surface openings. Ultrasonic and radiographic methods examine the interior, with different sensitivity to planar flaws. Sectioning and macro-etching show the interface directly on samples.
Visual inspection has a clear limit. It can see lack of fusion that breaks out at a toe or root surface, and it can see symptoms such as a cold, rolled-over edge. It cannot see buried interfaces. A visual report should say what it can and cannot clear.
Surface methods extend visual inspection slightly. Penetrant testing draws dye into fine openings, revealing surface-breaking flaws that are hard to see. Magnetic particle testing works on ferromagnetic steels. Neither reaches buried flaws, and penetrant is unsuitable for some surfaces.
Internal methods vary. Radiography is good at volumetric flaws such as porosity, but planar flaws aligned poorly with the beam can be hard to see. Ultrasonic testing is often more sensitive to planar flaws such as lack of fusion, but thin sections and small hardware joints limit its practicality. The specification should name the method suited to the joint.
Sectioning is the most direct method for small hardware joints. Cutting through a joint, grinding, polishing and etching the face shows where weld metal bonded and where it did not. It destroys the sample, so it is used for procedure qualification, first article review, periodic audits and disputes.
Destructive tests used in procedure qualification, such as bend tests on test coupons, can also expose lack of fusion by opening the unbonded face. Those tests belong to the welding procedure and its qualification records rather than routine lot inspection.
- Name the examination method on every report.
- State what the method can and cannot detect.
- For buried interfaces, rely on the method the specification requires, or sectioned samples.
- For small hardware joints, agree a sectioning plan rather than assume internal methods are practical.
- Keep procedure qualification records separate from lot inspection records.
What should a QC sheet record when lack of fusion is found?
Record the joint, the interface affected, its approximate length or extent, how it was found, the specimen or sample identity and the acceptance reference. Add a photo of the section or indication with a scale reference. That gives the supplier something specific to investigate and lets a reviewer apply the specified criteria.
Joint identification should use the drawing. The live guide on how to read welding symbols explains how drawings identify weld locations and types. Matching those identifiers in the QC record avoids confusion when several similar joints exist on one part.
Interface identification is the core field. Say whether the unbonded line is along the tube side or plate side of a fillet, between passes, or at the root. A section photo makes that unambiguous.
Extent describes how much was affected. On a section, record the length of the unbonded line relative to the joint. On internal examination, record the indication length the method reports. Avoid converting one into the other without the procedure.
Etching conditions should be noted for sections. Etchants reveal the boundary between weld metal and base metal; a faint, unclear boundary can make a well-fused joint look questionable, or hide a narrow unbonded line. Recording the preparation and etchant lets another laboratory reproduce the section, which matters if the finding is disputed.
Sample identity connects the finding to production. Record which part, which lot and which welding station or date, if known. Lack of fusion that appears on one sample may or may not represent the lot, which is a sampling question the specification or agreement should address.
What decides acceptance, and how should causes be discussed?
Acceptance belongs to the criteria the drawing or customer specification names, together with its required examination method. Many standards treat lack of fusion strictly, but this page does not print limits, because they depend on the standard, quality level, joint type and thickness the specification selects.
Product function should inform how strictly fusion is examined. A decorative hook joint carrying a light towel is a different risk from a fold-down shelf hinge bracket or a grab-style rail. Buyers who explain the load case help the supplier and any laboratory choose a sensible sampling and examination plan, instead of applying one level of scrutiny to every joint.
If the drawing is silent on fusion and examination, agree requirements before production. That agreement might name a weld quality standard and level, a sectioning frequency for first articles and periodic audits, and how findings will be handled. Settling it in advance avoids disputes over method after a finding.
Cause discussion should stay labelled as inference. General welding knowledge associates lack of fusion with joint preparation that limits access, welding parameters that give too little energy for the joint, travel speed too high for the current, torch or electrode angle, surface contamination and, in some processes, arc deflection. Those are general associations, not a diagnosis of a specific lot.
Surface condition before welding is one area buyers can ask about directly. Mill scale, oxide, oil and protective films can interfere with wetting along a sidewall. Asking how parts are cleaned between forming and welding, and how long cleaned parts wait before welding, is a reasonable evidence request that does not assume any particular cause.
Thickness mismatch is another general factor on hardware. Joining a thin tube to a much thicker plate means the plate draws heat away quickly, and the thinner side melts first. Procedures address this with torch position, sequence and parameters. A buyer seeing repeated findings on one mismatched joint can reasonably ask how the procedure handles it.
Confirming a cause requires the welding procedure, the parameter records, fit-up information and the sectioned evidence. A photo alone cannot separate, for example, a fit-up gap from a parameter problem.
From Koitor’s manufacturing side, joint fit-up is often decisive on thin hardware. Tube ends cut and notched to sit tightly against a plate, and wire ends positioned consistently in fixtures, give the arc or beam a joint it can fuse reliably. That is why fixture and fit-up evidence can be as useful as parameter records when fusion is questioned.
When a section does show lack of fusion, a useful next step is to check whether the finding repeats. Sectioning the same joint on a few more parts from the same lot, and on parts from a different shift or fixture, shows whether the problem is isolated or systematic. That evidence shapes the response far better than a single slice.

Buyer checklist before calling a weld lack of fusion
- The finding is an unbonded interface, not a gas pore, groove or low profile.
- The affected interface is identified: sidewall, inter-run or root, and which side.
- Lack of penetration has been considered and recorded separately if present.
- The examination method is named, with its detection limits understood.
- A section or indication photo with scale reference is attached.
- Sample identity links to part, lot and, where known, station or date.
- The acceptance reference and required examination method are named.
- Any cause is labelled as inference until procedure and fit-up records are reviewed.
FAQ
What is lack of fusion in welding?
Lack of fusion is an unbonded interface where weld metal did not melt into and join the base metal or a previous pass. It can occur along a sidewall, between passes or at the root. It is often internal and planar, so visual inspection may not reveal it.
Is lack of fusion the same as lack of penetration?
No. Lack of fusion is a bonding failure at an interface. Lack of penetration means the weld did not reach the required depth through the joint, leaving the root unfilled. A weld can have one without the other, so each should be named separately.
Can visual inspection detect lack of fusion?
Only when it breaks the surface at a toe or root. Buried lack of fusion needs an internal examination method or sectioning. A visual report should state that it cannot clear a weld of internal lack of fusion.
How is lack of fusion checked on small hardware welds?
Sectioning sample joints, polishing and etching the face is often the most practical method on small tube and wire joints. It destroys the sample, so it is typically used for first articles, periodic audits and disputes, according to an agreed plan.
What causes lack of fusion?
General welding knowledge links it to joint access, insufficient energy for the joint, travel speed, torch angle, contamination and, in some processes, arc deflection. These are general inferences. Confirming a cause on a specific lot needs the procedure, parameter and fit-up records.
Is lack of fusion always rejectable?
Many standards treat it strictly, but the decision belongs to the criteria and quality level the specification names. This page does not give limits. Agree the criteria and the examination method before production so findings can be judged consistently.
Collaborez avec Koitor Hardware
Review weld and inspection wording on a drawing
Send the drawing, the weld callouts and the inspection and acceptance requirements your customer applies. We can review whether the wording names fusion and penetration requirements, the examination method and the acceptance reference clearly enough for welded hardware parts. We do not act as a welding inspector.
Fabrication pour compte de tiers / Marque de distributeur
Transformez ce guide d'approvisionnement en cahier des charges
Indiquez-nous le produit souhaité, ses dimensions, sa finition, la quantité commandée et vos exigences en matière d'emballage. Votre équipe recevra une analyse pratique de la faisabilité de la fabrication avant l'établissement du devis.